In addition to materials with very low melting points such as zinc and tin and cemented carbide, various metal materials (including copper and aluminum)
Pieces can be repaired.
1. Local wear and tear caused by equipment and mold during use.
2. Processing defects in the manufacturing process, such as trachoma pores, excessive size, corner damage, insufficient argon welding, etc.
3. The rust spots and other depressions in the cavity.
Model | Cold Welder |
---|---|
Rated Input | 220 1Ф |
Rated Input(KVA) | 11KVA 7.5KW |
No Load Max Vo(V) | 36V |
Initial Current(A) | 3~300A |
Pulse Current(A) | 3~300A |
Spot Current(A) | 10~300A |
Duty Cycle(%) | 40% |
Gas After-flow time(sec) | 0.002~0.5S |
Gas Pre-flow time(sec) | 0.001~0.5S |
Crater Control system | Yes/No |
Outline dimensions(CM)W*D*H | 49.5*26*34.5 |
Weight(KG) | 21KG |
Insulation Class | H |
Duty Cycle 100% | 190AMP |